Ultra Low-cement Thixotropic Castables
Ultra Low-cement Thixotropic Castables
Technical characteristics
Rate for grade | ||||||
---|---|---|---|---|---|---|
МКRТ-42 | МКRТ-45 | МКRTU-50 | МLТ-60 | МКТ-72 | МКТ-90 | |
Spec. 14-194-275-06 |
||||||
Mass fraction of baked substance,%: Al2O3, minimum Fe2O3, maximum |
3,0 |
2,5 |
1,5 |
1,5 |
1,3 |
1,0 |
Compressive strength, N/mm², minimum | 30 | 40 | 65 | 35 | 45 | 70 |
Open porosity, %, maximum | 24 | 22 | 19 | 20 | 21 | 22 |
Temperature of deformation under load,°C, minimum | 1400 | 1450 | 1460 | 1480 | 1500 | 1660 |
Thermal shock resistance, heat cycles, minimum | - | - | - | 30 | - | - |
Items are made in accordance with customer’s drawings.
Upon agreement with the consumer it is possible to produce ground products.